Electroless Nickel / Immersion Gold Process Technology for
immersion gold solution parameters are equal. This condition was previously observed1 on a nickel deposit of phosphorus that achieved a gold thickness of #181;m, while a nickel layer of phosphorus yielded a gold thickness of only #181;m. Although the tool used to measure the gold thickness is also limited in